- Database
- Experimentalists
- Date
- 2019-02-21
- Parent sample
- Mixture #4 (Mo 28% : An 36% : Do 18% : Gr 18%) - 50-100 µm
- Thickness
- 2.0 $\pm$ 0.2 $mm$
- Substrate material
- aluminum
- Substrate comments
- raw aluminum sample holder
- Comments
- named Mixture #4_h (50-100 µm)
- Temperature
- 290.0 $\pm$ 1.0 $K$
- Temperature max
- 410.0 $\pm$ 20.0 $K$
- Time at Tmax
- 120.0 $min$
- Type
- molecular gas
- Fluids
-
- $N_2$ 100.0 %
- Fluid temperature
- 290.0 $K$
- Fluid pressure
- 1.0 $mbar$
- Number
- 1
- Layers
-
- Mixture #4 heated - 50-100 µm , 2.0 $mm$
- Title
- heating
- Samples
- Sample
- Mixture #4 heated (Mo 28% : An 36% : Do 18% : Gr 18%) - 50-100 µm (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 on parent sample 2019-02-18 thermal heating and mixing of sample between 390 and 430K for about 2 hours removal of most interlayer water in phyllosilicates (NH4-montmorillonite and Antigorite)