- Database
- Experimentalists
- Date
- 2014-01-01
- Thickness
- 1.0 $\pm$ 0.5 $mm$
- Diameter
- 5.0 $mm$
- Mass
- 0.023 $\pm$ 0.006 $g$
- Temperature
- 10.0 $\pm$ 1.0 $K$
- Time at T
- 180.0 $min$
- Temperature max
- 293.0 $K$
- Type
- atomic gas
- Fluids
-
- $He$ 100.0 %
- Fluid temperature
- 10.0 $K$
- Fluid pressure
- 1.0 $bar$
- Number
- 1
- Layers
- Title
- mixing and compressing of PVP-coated Ag nanoparticles with BN
- Matters
- Sample
- Pellet of PVP-coated Ag nano-particles mixed with BN (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mixing Mixed BN and nanoparticles manually in mortar during 15 min #2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min