- Database
- Experimentalists
- Date
- 2012-10-01
- Thickness
- 2.0 $\pm$ 0.5 $mm$
- Diameter
- 5.0 $mm$
- Mass
- 0.0428 $\pm$ 0.0055 $g$
- Temperature
- 20.0 $\pm$ -268.1 $^{\circ}C$
- Temperature max
- 19.85 $^{\circ}C$
- Type
- ambient air
- Pressure
- 1.0 $bar$
- Number
- 1
- Layers
-
- Pellet of Co doped zinc oxide mixed with BN , 2.0 $mm$
- Title
- mixing and compressing Co doped zinc oxide with BN
- Matters
- Materials
- Sample
- Pellet of Co doped zinc oxide mixed with BN (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mixing Mixed in mortar during 15 min #2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min