Sample
Name
Pellet of Low crystallized xenotime YPO4 mixed with PVP
Date
2022-06-15
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
0.031 $g$
Temperature
20.0 $\pm$ 278.15 $K$
Temperature max
293.15 $K$
Type
atomic gas
Fluids
Fluid temperature
20.0 $K$
Fluid pressure
1.0 $bar$
Title
mixing and compressing Low crystallized xenotime YPO4 with PVP

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Low crystallized xenotime YPO4 mixed with PVP (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min