- 2009-10-29
- Provider
- LPG Nantes
- Thickness
- 1.0 $\pm$ 0.1 $cm$
- Diameter
- 5.0 $cm$
- Volume
- 20.0 $cm^3$
- Comments
- Powder of the internal part of the sample
- Temperature
- 291.0 $\pm$ 2.0 $K$
- Type
- ambient air
- Fluid temperature
- 291.0 $\pm$ 2.0 $K$
- Number
- 1
- Layers
-
- Ogaden Kebri Dehar basalt powder K3.1p , 1.0 $cm$
- Title
- grinding
- Samples
- Sample
- Ogaden Kebri Dehar basalt powder K3.1p (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mechanical grinding - Comments
- The powder was obtained by crushing the sample manually using an Abiche mortar to a grain size < 2 mm, then powdering it finely in an agate grinder. The obtained powder was then dry sieved to a grain size < 25 µm.