- Database
- Experimentalists
- Date
- 2023-01-01
- Provider
- IPAG
- Thickness
- 1.0 0.1
- Diameter
- 7.0
- Mass
- 40.0 5.0
- Substrate material
- anodized aluminum
- Temperature
- 80.0 -272.1
- Comments
- the measurements were done at T = 80°C to minimize the amount of adsorbed terrestrial water
- Type
- vacuum
- Fluid temperature
- 23.85 -2.721e+02
- Fluid pressure
- 5.0e-04
- Number
- 1
- Arrangement
- The sample holder is filled to the top with non-compacted sample powder
- Layers
-
- Niger CM2 chondrite , 1.0
- Title
- grinding a raw piece of Niger CM2 chondrite
- Matters
- Sample
- powder of bulk Niger CM2 chondrite (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation 2023-01-01 mechanical grinding manually into an agate mortar a raw piece of meteorite powdered sample not sieved to keep a large distribution of grain sizes