Sample
Name
Pellet of CoSO4.H2O mixed with BN
Date
2014-09-19
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Temperature
300.0 $\pm$ 278.15 $K$
Temperature max
293.15 $K$
Title
mixing and compressing CoSO4.H2O with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of CoSO4.H2O mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min