Sample
Name
Pellet of cadmium hydroxide mixed with BN
Date
2006-01-01
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Temperature
15.0 $\pm$ 5.0 $K$
Temperature max
293.0 $K$
Type
atomic gas
Fluids
Fluid temperature
15.0 $K$
Title
mixing and compressing cadmium hydroxide with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of cadmium hydroxide mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min