- Database
- Experimentalists
- Date
- 2021-07-07
- Provider
- Sigma-Aldrich
- Thickness
- 2.0 $\pm$ 0.5 $mm$
- Diameter
- 5.0 $mm$
- Mass
- 0.02 $g$
- Temperature
- 293.0 $\pm$ 5.0 $K$
- Temperature max
- 293.0 $K$
- Type
- ambient air
- Fluid temperature
- 293.0 $K$
- Fluid pressure
- 1.0 $bar$
- Number
- 1
- Layers
- Title
- mixing and compressing La(PO4) synthetized at 900°C with PVP
- Matters
- Materials
- Sample
- Pellet of La(PO4) synthetized at 900°C mixed with PVP (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mixing Mixed in mortar during 15 min #2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min