Layer
Name
Pellet of La(PO4) synthetized at 200°C mixed with PVP
Type of layer
pellet
Thickness
2.0  ± 0.5  mm
Mass
0.02 g
Texture
compact poor grained
Type of porosity
closed pores
Formation mode
pressing compact material
Temperature
293.0  K
Pressure
7500.0  None
Comments
Pressed with a manual hydraulic press up to 1.5tons during 1min.
Number
2
Arrangement
homogeneous mixing
Materials
  Name Arrangement Mass (g) Mass fraction Abundance comments
La(PO4) synthetized at 200°C 9e-05 0.0045
PVP powder 0.9955