- Database
- Experimentalists
- Date
- 2009-03-01
- Provider
- LPG Nantes
- Thickness
- 10.0 $\pm$ 1.0 $mm$
- Diameter
- 50.0 $mm$
- Temperature
- 291.0 $\pm$ 2.0 $K$
- Type
- ambient air
- Fluid temperature
- 291.0 $\pm$ 2.0 $K$
- Number
- 1
- Layers
-
- Ogaden Werder basalt W3.7 , 10.0 $mm$