Sample
Name
Pellet of W_metal mixed with BN
Date
2015-06-21
Provider
Prolabo
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Mass
0.027 ± 0.00504 g
Temperature
20.0 ± 5.0 C
Temperature max
20.0 C
Type
ambient air
Fluid temperature
20.0 C
Fluid pressure
1.0 bar
Title
mixing and compressing W_metal with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of W_metal mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min