Sample
Name
thenardite powder (36-50µm grains)
Date
2018-04-19
Thickness
3.0 ± 0.2 mm
Substrate material
aluminium
Temperature
125.0 ± 1.0 K
Type
purged air
Fluids
Fluid pressure
5.0 ± 2.0 mbar
Comments
a few mbar of dry air were introduced into the closed cell in order to ensure an effective thermal equilibrium of the powder sample and to avoid dehydration.
Number
1
Layers