Sample
Name
Pellet of cobalt oxide Co(II,III) mixed with BN
Date
2012-09-27
Provider
Strem Chemicals
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
0.0215 $\pm$ 0.0055 $g$
Temperature
20.0 $\pm$ -268.1 $^{\circ}C$
Temperature max
19.85 $^{\circ}C$
Title
mixing and compressing cobalt oxide Co(II,III) with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of cobalt oxide Co(II,III) mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min