- Thickness
- 1.0 $\pm$ 0.5 $mm$
- Diameter
- 5.0 $mm$
- Mass
- 0.035 $\pm$ 0.006 $g$
- Temperature
- 293.0 $\pm$ 2.0 $K$
- Temperature max
- 293.0 $K$
- Type
- ambient air
- Pressure
- 1.0 $atm$
- Number
- 1
- Layers
-
- Pellet of Renazzo CR chondrite mixed with BN , 1.0 $mm$
- Title
- mixing and compressing of Renazzo CR chondrite with BN
- Matters
- Sample
- Pellet of Renazzo CR chondrite mixed with BN (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mechanical grinding the bulk CR manually in mortar during 15 min #2 before layer formation mixing Mixing BN and grinded CR manually in mortar during 15 min #2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min