- Database
- Experimentalists
- Date
- 2019-06-01
- Provider
- IPAG
- Thickness
- 1.0 $\pm$ 0.1 $mm$
- Diameter
- 7.0 $mm$
- Mass
- 40.0 $\pm$ 5.0 $g$
- Substrate material
- anodized aluminum
- Temperature
- 80.0 $\pm$ -272.1 $^{\circ}C$
- Comments
- the measurements were done at T = 80°C to minimize the amount of adsorbed terretsrial water
- Type
- ambient air
- Fluid temperature
- 23.85 $\pm$ -2.721e+02 $^{\circ}C$
- Fluid pressure
- 1.0e-04 $mbar$
- Number
- 1
- Arrangement
- The sample holder is filled to the top with non-compacted sample powder
- Layers
-
- EET90628 UOC , 1.0 $mm$
- Title
- grinding a raw piece of EET90628 UOC
- Matters
- Sample
- powder of bulk EET90628 UOC (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation 2019-07-01 mechanical grinding manually into an agate mortar a raw piece of meteorite powdered sample not sieved to keep a large distribution of grain sizes