Sample
Name
Pellet of V2O4 mixed with BN
Date
2006-03-04
Provider
Sigma-Aldrich
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
1.0039 $\pm$ 0.0011 $g$
Temperature
300.0 $K$
Title
mixing and compressing V2O4 with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of V2O4 mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min