- Database
- Experimentalists
- Date
- 2007-01-01
- Provider
- IPAG
- Previous sample
- Smectite SWy-2 with 3.85% adsorbed-interlayer H2O
- Parent sample
- Smectite SWy-2 with 1.44% adsorbed-interlayer H2O
- Thickness
- 1.0 0.1
- Diameter
- 30.0
- Volume
- 700.0
- Mass
- 0.4707 0.0901
- Surface roughness
- low
- Substrate material
- aluminum anodized black
- Substrate comments
- depth 1mm
- Comments
- Mass of dry sample = 0.46g
- Temperature
- 243.1 0.5
- Time at T
- 0.0
- Temperature max
- 443.0
- Time at Tmax
- 600.0
- Comments
- Sample temperature error is mostly due to possible vertical temperature gradient in the sample. Temperature reading accuracy and stability is 0.1K - Small pressure applied during sample flattening with a spatula
- Number
- 1
- Arrangement
- The sample holder is filled to rim with the non-compacted sample powder
- Layers
- Title
- decrease pressure to mbar
- Materials
- Materials
- Processing steps
-
Step Chronology Date Type Process Changes #1 on parent sample 2007-01-01 fluid physical decrease pressure to mbar adding adsorbed/interlayer - Comments
- negligible adsorption assumed on the other materials