Layer
Name
Mixture of Tholins UARK 90N2 10CH4 with liqCH3CN and liqC2H6
Type of layer
various
Texture
muddy
Type of porosity
without pores
Comments
layer of tholins mixed with liquid C2H6 and liquid CH4
Formation mode
liquid drops on powder
Temperature
93.0  $K$
Comments
The sample is produced by progressive adding of drops of liquid CH3CN and liquid C2H6 on the tholins powder material manually deposited at the bottom of a Petri dish.
Number
3
Arrangement
grains in fluid
Materials
  Name Arrangement Mass (g) Mass fraction Abundance comments
Liquid C2H6 liquid C2H6 and liquid CH3CN wetting the tholins Tholins are flood by liquid C2H6
Liquid CH3CN liquid CH3CN wetting the tholins Tholins are flood by liquid CH3CN
Tholins UARK 90N2 10CH4 0.06 60 mg of tholins #2 were scratched from the surface of the two glass sections that were located in the sputterig machine for tholin genesis. In addition, the Spectralon used in the 2014 experiment was also located in the sputtering machine and collecting additional matter. That matter was stuck to the Spectralon and could not be weighted. The total mass of tholins #2 used in the 2014 experiment is 60 mg - granular matter loss during transfer to the surface of Spectralon + unweighted mass of matter deposited on Spectralon.