Layer
- Name
- Pellet of uraninite (UO2)
- Type of layer
- pellet
- Thickness
- 1.0 $\pm$ 0.5 $mm$
- Texture
- compact poor grained
- Type of porosity
- closed pores
- Formation mode
- pressing compact material
- Temperature
- 1800.0 $^{\circ}C$
- Comments
- Powder calcinated at 700°C, pressed and then sintered between 1500 and 1600°C. Protocole described in the associated publications.