Sample
Name
Pellet of La(PO4) synthetized at 900°C mixed with PVP
Date
2021-07-07
Provider
Sigma-Aldrich
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
0.02 $g$
Temperature
293.0 $\pm$ 5.0 $K$
Temperature max
293.0 $K$
Type
ambient air
Fluid temperature
293.0 $K$
Fluid pressure
1.0 $bar$
Title
mixing and compressing La(PO4) synthetized at 900°C with PVP

Precursors

Matters
Materials

Produced sample

Sample
Pellet of La(PO4) synthetized at 900°C mixed with PVP (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min