Layer
Name
Pellet of High crystallized xenotime YPO4 mixed with PVP
Type of layer
pellet
Thickness
2.0  $\pm$ 0.5  $mm$
Mass
0.0322 $g$
Texture
compact poor grained
Type of porosity
closed pores
Formation mode
pressing compact material
Temperature
293.0  $^{\circ}C$
Pressure
7500.0  $None$
Comments
Pressed with a manual hydraulic press up to 1.5tons during 1min.
Number
2
Arrangement
homogeneous mixing
Materials
  Name Arrangement Mass (g) Mass fraction Abundance comments
High crystallized xenotime YPO4 0.0056 0.173913043478261
PVP powder 0.826086956521739