Sample
Name
Pellet of Y-doped hematite mixed with PVP
Date
2022-06-15
Thickness
2.0 ± 0.5 mm
Diameter
5.0 mm
Temperature
20.0 ± 5.0 C
Temperature max
20.0 C
Type
ambient air
Fluid temperature
20.0 C
Fluid pressure
1.0 bar
Title
mixing and compressing Y-doped hematite with PVP

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Y-doped hematite mixed with PVP (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min