Sample
Name
powder of bulk MIL07193 CO chondrite
Date
2019-06-01
Provider
IPAG
Thickness
1.0 $\pm$ 0.1 $mm$
Diameter
7.0 $mm$
Mass
40.0 $\pm$ 5.0 $g$
Substrate material
anodized aluminum
Temperature
297.0 $\pm$ 1.0 $K$
Type
ambient air
Fluid temperature
297.0 $\pm$ 1.0 $K$
Fluid pressure
1.0e-04 $mbar$
Number
1
Arrangement
The sample holder is filled to the top with non-compacted sample powder
Layers
Title
grinding a raw piece of MIL07193 CO chondrite

Precursors

Matters

Produced sample

Sample
powder of bulk MIL07193 CO chondrite (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation 2019-07-01 mechanical grinding manually into an agate mortar a raw piece of meteorite powdered sample not sieved to keep a large distribution of grain sizes