Sample
Name
powder of bulk MIL090657 CR chondrite
Date
2019-01-01
Provider
IPAG
Thickness
2.0 0.1
Diameter
13.0
Mass
50.0 5.0
Substrate material
anodized aluminum
Temperature
297.0 1.0
Type
ambient air
Fluid temperature
297.0 1.0
Fluid pressure
1.0
Number
1
Arrangement
The sample holder is filled to the top with non-compacted sample powder
Layers
Title
grinding a raw piece of MIL090657 CR chondrite

Precursors

Matters

Produced sample

Sample
powder of bulk MIL090657 CR chondrite (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation 2019-01-01 mechanical grinding manually into an agate mortae a raw piece of meteorite powdered sample not sieved to keep a large distribution of grain sizes