- Database
- Experimentalists
- Date
- 2022-11-14
- Provider
- LESIA
- Thickness
- 2.0 ± 0.1 mm
- Diameter
- 13.0 mm
- Mass
- 50.0 ± 5.0 g
- Substrate material
- anodized aluminum
- Temperature
- 297.0 ± 1.0 K
- Type
- ambient air
- Fluid temperature
- 297.0 ± 1.0 K
- Fluid pressure
- 1.0 bar
- Number
- 1
- Arrangement
- The sample holder is filled to the top with non-compacted sample powder
- Layers
-
- CH-rich-20 , 2.0 mm
- Title
- Crushing and sieving of DECS19 and mixing with PSD in the right volumetric proportion
- Matters
- Sample
- CH-rich-20 (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation 2022-11-14 mechanical crushing of DECS19 and sieving to select the grain size 50 - 100 μm #2 before layer formation 2022-11-14 mechanical mixing of PSD (80 vol.%) and DECS19 (20 vol.%)