Sample
Name
Tagish Lake KBr pellet
Date
2023-01-01
Provider
IPAG
Thickness
0.8 $\pm$ 0.1 $mm$
Diameter
13.0 $mm$
Mass
0.301 $\pm$ 0.0011 $g$
Substrate material
sample holder in aluminum with a centered hole to hold the sample
Comments
KBr pellet of 13mm of diameter and 0.8mm thick
Temperature
22.0 $\pm$ 2.0 $^{\circ}C$
Temperature max
22.0 $\pm$ 2.0 $^{\circ}C$
Type
vacuum
Fluid pressure
0.001 $mbar$
Comments
stored in a desiccator
Title
Grinding of the Tagish Lake meteorite, mixing with KBr, pellet making

Precursors

Matters

Produced sample

Sample
Tagish Lake KBr pellet (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation 2023-01-01 mechanical grinding bulk meteorite reduced to grains with size lower than 10 microns
#2 before layer formation 2023-01-01 thermal 300 mg of commercial ultrapure KBr powder was heated under ambient air to 80°C overnight (~10h) removal of adsorbed/hydration water in KBr powder
#3 before layer formation 2023-01-01 mixing homogeneous mixing 1.0 mg of grinded meteorite was weighed and mixed with 300 mg of dried commercial ultrapure KBr powder
#4 during layer formation 2023-01-01 pressure pressure formation of a pellet of 13mm diameter and 0.8 mm thick under 400 bars of pressure