- Database
- Experimentalists
- Date
- 2022-09-01
- Provider
- JAXA
- Thickness
- 10.0 ± 10.0 μm
- Diameter
- 50.0 μm
- Substrate material
- synthetic type IIa diamond windows
- Substrate comments
- 3 x 0.5 mm diamond windows
- Comments
- manual selection under binocular of about 10 fragments of approximate diameter of 30-50 microns
- Temperature
- 22.0 ± 2.0 ∘C
- Temperature max
- 22.0 ± 2.0 ∘C
- Comments
- HYB2 samples stored under N2
- Type
- ambient air
- Fluid pressure
- 1.0 atm
- Number
- 1
- Layers
-
- C0050 fragments , 10.0 μm
- Title
- selection and pressing of the grains
- Matters
- Sample
- C0050 fragments (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mechanical Manual selection of one or several fragment(s) of C0050 in a glove box filled with N2. The main C0050 particule was kept under N2 in a specific container and the selected fragments were then micro-manipulated under ambient air #2 during layer formation mechanical Fragments pressed between two synthetic type IIa diamond windows with a mechanical press - ambient air fragments pressed between two diamond windows - unknown thickness