- Database
- Experimentalists
- Date
- 2023-05-23
- Provider
- LESIA
- Thickness
- 2.0 $\pm$ 0.1 $mm$
- Substrate material
- anodized aluminum
- Temperature
- 297.0 $\pm$ 1.0 $K$
- Type
- purged air
- Fluid temperature
- 297.0 $\pm$ 1.0 $K$
- Fluid pressure
- 1.0 $bar$
- Number
- 1
- Arrangement
- The sample holder is filled to the top with non-compacted sample powder
- Layers
-
- hydmin-rich-15 , 2.0 $mm$
- Title
- Mixing of PSD and antigorite in the right volumetric proportion
- Matters
- Sample
- hydmin-rich-15 (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation 2023-05-22 mechanical mixing of PSD (85 vol.%) and antigorite (15 vol.%)