Sample
Name
Pellet of Vanadyl acetylacetonate C10H14O5V mixed with BN
Date
2022-03-01
Provider
Sigma-Aldrich
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
1.0125 $g$
Temperature
20.0 $\pm$ 5.0 $^{\circ}C$
Temperature max
20.0 $^{\circ}C$
Type
ambient air
Fluid temperature
20.0 $^{\circ}C$
Fluid pressure
1.0 $bar$
Title
mixing and compressing Vanadyl acetylacetonate C10H14O5V with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of Vanadyl acetylacetonate C10H14O5V mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min