- Database
- Experimentalists
- Date
- 2023-01-01
- Provider
- Institut d'Astrophysique Spatial, Orsay, France
- Thickness
- 3.0 $\pm$ 0.5 ${\mu}m$
- Substrate material
- Diamond
- Comments
- Grain crushed inside a diamond compression cell
- Temperature
- 20.0 $\pm$ 10.0 $^{\circ}C$
- Temperature max
- 30.0 $\pm$ 5.0 $^{\circ}C$
- Type
- ambient air
- Fluid temperature
- 20.0 $\pm$ 10.0 $^{\circ}C$
- Fluid pressure
- 1.0 $atm$
- Number
- 1
- Layers
-
- IDP L2079 J1 , 3.0 ${\mu}m$
- Title
- IDP 2079 J1 preparation
- Matters
- Sample
- IDP L2079 J1 (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 during layer formation 2014-01-01 mechanical mechical crushing of the IDP L2079 J1 in the diamond compression cell - Comments
- The sample was crushed into a diamond compression cell until obtain a maximum thickness of 3 µm.