- Database
- Experimentalists
- Date
- 2016-08-31
- Provider
- IAS, Orsay
- Thickness
- 3.0 $\pm$ 0.5 ${\mu}m$
- Diameter
- 40.0 ${\mu}m$
- Mass
- 1.8e-08 $\pm$ 1e-07 $g$
- Substrate material
- Diamond
- Comments
- Grain crushed inside a diamond compression cell
Hyper-spectrale MIR spectroscopy of Paris meteorite in tranmission (sample crushed in a diamand compression cell)
- Temperature
- 300.0 $\pm$ 5.0 $K$
- Temperature max
- 300.0 $\pm$ 5.0 $K$
- Type
- ambient air
- Fluid temperature
- 300.0 $K$
- Fluid pressure
- 1032.0 $hPa$
- Number
- 1
- Layers
-
- Grain_ZED , 3.0 ${\mu}m$
- Title
- Paris grain preparation
- Matters
- Sample
- Grain_ZEDGrain of Paris meteorite (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 during layer formation 2016-08-31 mechanical mechical crushing of the Paris grain in the diamon compression cell - Comments
- The sample was crushed into a diamond compression cell until obtain a maximum thickness of 3 µm.