Material
Name
Co doped aluminum oxide
Family
solid
Origin
laboratory
Comments
Prepared by thermal decomposition of a powder mixture of Al(OH)3 and Co(NO3)2.6H2O at 1000°C in air for 12h (sweep rate of +4°C/min for the heating stage). The Co/Al atomic ratio in the precursors mixture is 0.01.
Relevance
main - major
Mass
0.0303 $\pm$ 0.0005 $g$
Mass fraction
0.742647058823529 $\pm$ 0.112366637831603
Number
2
Arrangement
single phase
  Name Compound type Arrangement Mass ($g$) Mass fraction Adsorbat name
Aluminum oxide oxide single phase 0.9945 $\pm$ 0.0001
Cobalt elemental solid single phase 0.0055 $\pm$ 0.0001