Material
Name
Co doped zinc oxide
Family
solid
Origin
laboratory
Comments
Prepared by thermal treatment of a powder mixture of ZnO and Co(Cl)2.6H2O at 1000°C in air for 12h (sweep rate of +4°C/min for the heating stage). The Co/Zn atomic ratio in the precursors mixture is 0.008.
Relevance
main - major
Mass
0.0321 $\pm$ 0.0005 $g$
Mass fraction
0.75 $\pm$ 0.108060747663551
Number
2
Arrangement
single phase
  Name Compound type Arrangement Mass ($g$) Mass fraction Adsorbat name
Zinc oxide oxide-hydroxide single phase 0.9973 $\pm$ 0.0001
Cobalt elemental solid single phase 0.0027 $\pm$ 0.0001