- Database
- Experimentalists
- Date
- 2013-09-02
- Thickness
- 1.0 0.5
- Diameter
- 5.0
- Mass
- 0.0475 0.0075
- Temperature
- 293.0 5.0
- Temperature max
- 293.0
- Type
- ambient air
- Fluid temperature
- 293.0
- Fluid pressure
- 1.0
- Number
- 1
- Layers
- Title
- mixing and compressing of WIS91600 CM chondrite with BN
- Matters
- Sample
- Pellet of WIS91600 CM chondrite mixed with BN (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation mechanical grinding the bulk CM manually in mortar during 15 min #2 before layer formation mixing Mixing BN and grinded CM manually in mortar during 15 min #2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min