Sample
Name
matrix fragments
Date
2019-05-01
Provider
IPAG
Thickness
15.0 $\pm$ 1.0 ${\mu}m$
Diameter
40.0 ${\mu}m$
Substrate material
diamond window
Substrate comments
diamond window of 3.5mm diameter
Comments
manual selection under binocular of about 10 matrix grains of approximate diameter between 30 and 50 microns
Temperature
22.0 $\pm$ 2.0 $^{\circ}C$
Number
1
Layers
Title
selection of matrix fragments

Precursors

Matters

Produced sample

Sample
matrix fragments (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation 2019-05-01 mechanical Manual selection under optical binocular of about 10 matrix grains of about 30-50 microns diameter. Matrix selected based on its black color and on its fine-grained texture
#2 during layer formation 2019-05-01 mechanical fragments pressed between two diamond windows with a mechanical press fragments crushed down to a thickness of about 10 microns