Sample
Name
anthracite
Date
2022-06-04
Provider
LESIA
Thickness
2.0 $\pm$ 0.1 $mm$
Substrate material
anodized aluminum
Temperature
297.0 $\pm$ 1.0 $K$
Type
purged air
Fluid temperature
297.0 $\pm$ 1.0 $K$
Fluid pressure
1.0 $bar$
Number
1
Arrangement
The sample holder is filled to the top with non-compacted sample powder
Layers
Title
Crushing and sieving of the anthracite sample

Precursors

Matters

Produced sample

Sample
anthracite (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation 2022-04-06 mechanical grinding DECS19 was ground using a cryogenic grinder Retsch Cryomill at LGPM (Laboratoire Génie des Procédés et Matériaux, France)
#2 before layer formation 2022-04-06 mechanical sieving dry-sieving and selection of the size range of the grain 50 - 100 μm