Pb L3 edge XAS transmission of lead oxide litharge PbO at ambient conditions
- Title
- Pb L3 edge XAS transmission of lead oxide litharge PbO at ambient conditions
- DOI
- 10.26302/SSHADE/EXPERIMENT_DT_20170215_000
- Data reference
- Testemale, Denis; Brugger, Joel; Etschmann, Barbara; Liu, Weihua (2017): Pb L3 edge XAS transmission of lead oxide litharge PbO at ambient conditions. SSHADE/FAME (OSUG Data Center). Dataset/Spectral Data. https://doi.org/10.26302/SSHADE/EXPERIMENT_DT_20170215_000
- Publications
- Database
- Experimentalists
- Experiment type
- laboratory measurement
- Type
- transmission
- Intensity unit
- AU
- Instrument
- X-ray Absorption Spectroscopy measured in transmission mode
- Sample holder
- simple holder
- Standard medium
- unknown
- Observation mode
- spectrum
- Spectral range type(s)
- hard X
- Valid spectral range(s)
-
Min - Max ($eV$) Sampling ($eV$) Resolution ($eV$) Position accuracy ($eV$) Absorption edge #1 12847.0 - 14000.0 0.668 $Pb$ (L3: 13.0352 $keV$) - Comments
- poor data quality
Definition: incidence and emergence angles are positive with origin at nadir. Emergence angle in transmission is larger than 90° (=180°-i).
- Observation geometry
- direct
- Observation mode
- fixed angles
- Observation mode
- single spot
- Experiment
- Pb L3 edge XAS transmission of lead oxide litharge PbO at ambient conditions
- Date begin
- 2017-02-15
- Release date
- 2022-10-05 20:40:20 UTC+0000
- Version (Date)
- #1 (2022-10-05 20:40:20 UTC+0000, Updated: 2022-10-05 20:40:20 UTC+0000)
- History
-
Date Mode Version Status Comments 2022-10-05 20:38:04 UTC+0000 first import #1 valid version
- Analysis
- raw averaged spectra