- Database
- Experimentalists
- Date
- 2022-06-04
- Provider
- LESIA
- Thickness
- 2.0 $\pm$ 0.1 $mm$
- Substrate material
- anodized aluminum
- Temperature
- 297.0 $\pm$ 1.0 $K$
- Type
- purged air
- Fluid temperature
- 297.0 $\pm$ 1.0 $K$
- Fluid pressure
- 1.0 $bar$
- Number
- 1
- Arrangement
- The sample holder is filled to the top with non-compacted sample powder
- Layers
-
- anthracite , 2.0 $mm$
- Title
- Crushing and sieving of the anthracite sample
- Matters
- Sample
- anthracite (this sample)
- Processing steps
-
Step Chronology Date Type Process Changes #1 before layer formation 2022-04-06 mechanical grinding DECS19 was ground using a cryogenic grinder Retsch Cryomill at LGPM (Laboratoire Génie des Procédés et Matériaux, France) #2 before layer formation 2022-04-06 mechanical sieving dry-sieving and selection of the size range of the grain 50 - 100 μm