Sample
Name
Pellet of synthetic zircon ZrSiO4 mixed with BN
Date
2009-11-01
Provider
Sigma Aldrich
Thickness
1.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Temperature
293.0 $\pm$ 2.0 $K$
Temperature max
293.0 $K$
Type
ambient air
Fluid temperature
293.0 $K$
Fluid pressure
1.0 $bar$
Title
mixing and compressing of synthetic zircon ZrSiO4 with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of synthetic zircon ZrSiO4 mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed BN and zircon manually in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min