Sample
Name
Pellet of ZnS Zn sulfide sphalerite mixed with BN
Date
2018-04-18
Provider
Sigma-Aldrich
Thickness
2.0 $\pm$ 0.5 $mm$
Diameter
5.0 $mm$
Mass
0.2123 $g$
Temperature
10.0 $\pm$ 5.0 $K$
Temperature max
293.0 $K$
Title
mixing and compressing ZnS Zn sulfide sphalerite with BN

Precursors

Matters
Materials

Produced sample

Sample
Pellet of ZnS Zn sulfide sphalerite mixed with BN (this sample)
Processing steps
Step Chronology Date Type Process Changes
#1 before layer formation mixing Mixed in mortar during 15 min
#2 during layer formation pressure Pressed with a manual hydraulic press up to 1.5 tons during 1 min